Rajiv Mukherjee

Prime Minister's Research Fellow, Department of Earth Sciences, Indian Institute of Technology Kanpur, India

Nanomechanics of minerals: understandings and developments through instrumented nanoindentation techniques


Journal article


Rajiv Mukherjee, Santanu Misra
Physics and Chemistry of Minerals, vol. 50(1), 2023, pp. 1-33


View PDF
Cite

Cite

APA   Click to copy
Mukherjee, R., & Misra, S. (2023). Nanomechanics of minerals: understandings and developments through instrumented nanoindentation techniques. Physics and Chemistry of Minerals, 50(1), 1–33. https://doi.org/10.1007/s00269-023-01235-8


Chicago/Turabian   Click to copy
Mukherjee, Rajiv, and Santanu Misra. “Nanomechanics of Minerals: Understandings and Developments through Instrumented Nanoindentation Techniques.” Physics and Chemistry of Minerals 50, no. 1 (2023): 1–33.


MLA   Click to copy
Mukherjee, Rajiv, and Santanu Misra. “Nanomechanics of Minerals: Understandings and Developments through Instrumented Nanoindentation Techniques.” Physics and Chemistry of Minerals, vol. 50, no. 1, 2023, pp. 1–33, doi:10.1007/s00269-023-01235-8.


BibTeX   Click to copy

@article{rajiv2023a,
  title = {Nanomechanics of minerals: understandings and developments through instrumented nanoindentation techniques},
  year = {2023},
  issue = {1},
  journal = {Physics and Chemistry of Minerals},
  pages = {1-33},
  volume = {50},
  doi = {10.1007/s00269-023-01235-8},
  author = {Mukherjee, Rajiv and Misra, Santanu}
}